Rubber internal release agent, which improves the release effect.
Test Items | Test Results |
Appearance | Pale yellow or creamy white cylindrical (or hemispherical) granules |
Melting Point | 80~120 ℃ |
Ash | ≤ 8.5 % |
Heating Loss | ≤ 3.0 % |
Properties: A mixture of saturated fatty acids, high molecular weight silicone resins and high carbon alcohols.
Performance: An internal mold release agent for rubber and rubber-plastic materials with internal and external lubricity and mold release functions. Can be used for complex molds and injection molded vulcanized products to improve the fluidity of the rubber compound in the mold and reduce the probability of quality defects.
Application: Mainly be used in the production of natural rubber, all kinds of unsaturated synthetic rubber (except fluorine rubber and silicone rubber) and all kinds of thermoplastic elastomer products, such as tires, hoses and tapes, dams, etc.